Author Topic: Brass Etching - chemical residue  (Read 2028 times)
christoffer
Snr. Officer
****
Denmark Denmark



« on: January 30, 2011, 05:44:54 pm »

Hello! this is something that ive been wondering, if you are etching brass in salt water, the chloride ions and copper/zinc ions in brass will form CuCl2 and ZnCl2 as far as i remember, those salts i believe is harmfull and/or hazardrous for the environment, what do you do with the residue etching saltwater solution full of CuCl2 and ZnCl2 ?
give it to a recycling station or?
Logged
von Corax
Squire of the Lambda Calculus
Moderator
Immortal
*
Canada Canada

Prof. Darwin Prætorius von Corax


« Reply #1 on: January 31, 2011, 05:29:30 am »

I'd mix it with a good dose of washing soda (sodium carbonate, Na2CO3), then let it stand overnight. The reaction gives you copper (II) carbonate (CuCO3) and zinc carbonate (ZnCO3), both of which will precipitate out as a solid, and sodium chloride.
Logged

By the power of caffeine do I set my mind in motion
By the Beans of Life do my thoughts acquire speed
My hands acquire a shaking
The shaking becomes a warning
By the power of caffeine do I set my mind in motion
The Leverkusen Institute of Paleocybernetics is 5838 km from Reading
Pages: [1]   Go Up
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.20 | SMF © 2013, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.024 seconds with 17 queries.